Oct 14, 2010 #1 rscassar Structural Joined Jul 29, 2010 Messages 631 Location AU Does anyone know what joint design group to use for Hyne LVL members? I am doing a bolted connection to AS1720. Thanks and regards.
Does anyone know what joint design group to use for Hyne LVL members? I am doing a bolted connection to AS1720. Thanks and regards.
Oct 14, 2010 #2 rowingengineer Structural Joined Jun 18, 2009 Messages 2,476 Location AU You need to refer to manufacture spec, you can get many different grades of LVL. A clear conscience is usually the sign of a bad memory Upvote 0 Downvote
You need to refer to manufacture spec, you can get many different grades of LVL. A clear conscience is usually the sign of a bad memory
Oct 14, 2010 #3 apsix Structural Joined Sep 21, 2004 Messages 1,358 Location AU As he said, but it's typically JD4 for radiata pine LVL. Upvote 0 Downvote
Oct 16, 2010 Thread starter #4 rscassar Structural Joined Jul 29, 2010 Messages 631 Location AU The design in hyne program says JD3. Upvote 0 Downvote
Oct 16, 2010 #5 rowingengineer Structural Joined Jun 18, 2009 Messages 2,476 Location AU Can't help you to much in my area they only supply LGL and did away with LVL. A clear conscience is usually the sign of a bad memory Upvote 0 Downvote
Can't help you to much in my area they only supply LGL and did away with LVL. A clear conscience is usually the sign of a bad memory
Oct 17, 2010 #6 apsix Structural Joined Sep 21, 2004 Messages 1,358 Location AU The latest Tilling advice is down to JD5 for fixing parallel to the glue lines (rad pine LVL). You need to be confident that the specified manufacturer will be used on site if using the higher strength group. Upvote 0 Downvote
The latest Tilling advice is down to JD5 for fixing parallel to the glue lines (rad pine LVL). You need to be confident that the specified manufacturer will be used on site if using the higher strength group.
Oct 17, 2010 Thread starter #7 rscassar Structural Joined Jul 29, 2010 Messages 631 Location AU What does everyone think about using recycled timber? Say some wood trusses were brought down from site, before that timber can be reused, does it need to go away for treatment and grading? Upvote 0 Downvote
What does everyone think about using recycled timber? Say some wood trusses were brought down from site, before that timber can be reused, does it need to go away for treatment and grading?