Jan 17, 2017 #1 stan000 Mechanical Joined Jul 31, 2014 Messages 121 Location CA what is Minimum P.T.dwell time of weld as per ASME I THINK As per ASME section V Table 2 STEEL MATERIAL ON WELD Penetrate time shows 5 min. please let me know i am wrong or right. regards stanly
what is Minimum P.T.dwell time of weld as per ASME I THINK As per ASME section V Table 2 STEEL MATERIAL ON WELD Penetrate time shows 5 min. please let me know i am wrong or right. regards stanly
Jan 18, 2017 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Yes, it is 5 minutes per Table T-672 for metal temperature at 50 deg F to 125 deg F. Upvote 0 Downvote
Jan 18, 2017 Thread starter #3 stan000 Mechanical Joined Jul 31, 2014 Messages 121 Location CA Thanks. Regards stanly Upvote 0 Downvote