On my 1st Gen Tundra, lower BJ failures are common. So common that it is standard practice to replace them with OEM every 100k miles. Toyota had a recall and improved the joints but the failures persist.
Seems the issue is the suspension is designed so the joint is in tension. Spring/shock attached to LCA, stud pointing downwards.
Is it common to design suspension like that? It would seem having the joint in compression would be safer.
 
It is not- most (modern) double wishbone suspension designs will have the LBJ in compression.

The only two applications I am aware of are the Tundra and some generations of the Honda Accord.
 
Lots of older suspension designs were that way. The traditional American-car upper and lower wishbone suspensions with the spring acting on the lower control arm were that way for decades. All of the Ford Fox body cars, Mustang, Fairmont, etc (MacPherson, but with the spring separate from the strut and acting on the control arm) were that way.
 
Up until a couple of decades ago there was no recommendation either way. Then a whole bunch of manufacturers ran into durability failures in service that hadn't shown up in testing. In at least one case it turns out the boot manufacturer had surreptitiously changed the material used for the boot over the joint, to the extent it no longer met the rig test KPI. Once the boot cracks, water and grit get in, lubricant comes out. So long as your boot isn't cracked you should be OK.

I am told the ball joints themselves aren't a serviceable item on some SUVs, you have to buy a whole new arm.
 
Right, we've had to replace the lower ball joints/ control arms on the van twice allready in the last 4 years.. I think next time instead of buying just the ball joints installe don the control arm , we'll get the control arm that has the option to installed new ball joints whenever one is needed and keep the may control arm if deemed worthy of being kept.. Look into thing like the mevotech control arms with removable or adjustable lower ball joints. this way it would be a much easier installed. I've even went as far as to installed thing like mevotechs "over engineered" products on the van.
 
Lots of older suspension designs were that way. The traditional American-car upper and lower wishbone suspensions with the spring acting on the lower control arm were that way for decades. All of the Ford Fox body cars, Mustang, Fairmont, etc (MacPherson, but with the spring separate from the strut and acting on the control arm) were that way.
Do they all have the ball joint facing in the direction so it is in tension?
 
Several years ago My older daughter's 1996 Honda Accord had a lower ball joint break/unseat while slowly navigating her residential neighborhood.
That car had passed Massachusetts' annual RMV inspection about a month before.
It was the OEM joint with over100 kmiles.

Replacing front brake rotors on that car required substantial and unexpected suspension disassembly, made a way bigger project thanks to several years of Massachusetts road salt corrosion.

Despite those details I still hold Honda engineering in high regard.
 
Several years ago My older daughter's 1996 Honda Accord had a lower ball joint break/unseat while slowly navigating her residential neighborhood.
That car had passed Massachusetts' annual RMV inspection about a month before.
It was the OEM joint with over100 kmiles.

Replacing front brake rotors on that car required substantial and unexpected suspension disassembly, made a way bigger project thanks to several years of Massachusetts road salt corrosion.

Despite those details I still hold Honda engineering in high regard.
Anecdotally I believe these failures occur more frequently at low speed because:
  • More weight on the front wheels
  • Generally more turning/ball joint rotation
I've never looked into it but it makes sense to me intuitively.

The Accord suspension is certainly flawed from a design standpoint- not only is the lower ball joint in tension, but it requires significant disassembly to replace. You have to separate the knuckle/bearing from the CV shaft to even access the ball joint. At least the Toyota ball joint is bolted on- much easier to replace.
 
Interestingly, this ball joint incorporates a sintered bearing (and zerk)- a significant departure from the sealed polymer bearings that are in use today. Maybe the fact that it's facing upwards will mitigate grease starvation, but otherwise I'd be concerned about potential adhesion between bearing and housing.
 
Anecdotally I believe these failures occur more frequently at low speed because:
  • More weight on the front wheels
  • Generally more turning/ball joint rotation
I've never looked into it but it makes sense to me intuitively.

The Accord suspension is certainly flawed from a design standpoint- not only is the lower ball joint in tension, but it requires significant disassembly to replace. You have to separate the knuckle/bearing from the CV shaft to even access the ball joint. At least the Toyota ball joint is bolted on- much easier to replace.
This tool made it easy to replace the the VERY rusty Accord's Ball joints.

 