I am wondering what is the definition of "Low Temperature Service". For example, what is the max temperature that a ASTM A420 Grade WPL6 elbow can be used? How do the chemistry and mechanical properties differ from non-low temp service?

Thanks in advance

 
has to do with low temperature embrittlement
 
The definition of low temperature service refers to service temperature below ambient, and is based on Charpy impact requirements. ASME SA 420 states the following;

at -50 deg F, the minimum Charpy impact value is 13 ft-lbs for WPL6 material (see Tables 5 and 6).

Materials used for low temperature service have deliberate alloy additions and/or heat treatments to enhance fracture toughness at low service temperatures. In addition, fine grained melting practice improves low temperature service.
 
Thanks for the explanation.

Do these low temperature materials also have a upper temperature limit?
 
Yes. The upper temperature limit is defined in ASME Section II Part D. For WPL6, which is a carbon steel, the allowable stress value (17.1 Ksi) remains consistent to 650 deg F. Above this temperature, the allowable stress starts to decrease to 8.5 Ksi at 850 deg F (the maximum service temperature).
 