What type of pipe & fittings used in LPG tank at very low temperature, -60 degrees. Any specified material / brand?
 
9% Nickel steel


A844/A844M-93(1999) Standard Specification for Steel Plates, 9% Nickel Alloy, for Pressure Vessels, Produced by the Direct-Quenching Process

A522/A522M-01 Standard Specification for Forged or Rolled 8 and 9% Nickel Alloy Steel Flanges, Fittings, Valves, and Parts for Low-Temperature Service

A961-02 Standard Specification for Common Requirements for Steel Flanges, Forged Fittings, Valves, and Parts for Piping Applications

A553/A553M-95(2000) Standard Specification for Pressure Vessel Plates, Alloy Steel, Quenched and Tempered 8 and 9 Percent Nickel

A353/A353M-93(1999) Standard Specification for Pressure Vessel Plates, Alloy Steel, 9 Percent Nickel, Double-Normalized and Tempered




 
Any recommended BRAND for Low Temperature pipe for LPG at below-60 degrees.
 