I am seeking sources for low-temperature phase-change (-10 degrees C to -40 degrees C) materials, or formualae to produce them ourselves. I can find very little in the literature regarding this subject.

Regards, Winthrop
 
Dear Friend

You are advised to go through Chapter-2 of the book 'Cryogenic System' by R. Barron, Oxford University Press 1985.
Good luck.
 