Dear Experts,
I'm designing a system where a reactor is cooled using liquid nitrogen inside a jacket around the reactor. The boilig point of liquid N2 at atmospheric pressure is about -196 deg C. I'm sure that the SS 304/316 could not be used at this low temp. I'm certain, it gotta be low some grade of low temperature carbon steel.
Can you throw some light on the material selection??
Thanks in advance,
Timewrap.
I'm designing a system where a reactor is cooled using liquid nitrogen inside a jacket around the reactor. The boilig point of liquid N2 at atmospheric pressure is about -196 deg C. I'm sure that the SS 304/316 could not be used at this low temp. I'm certain, it gotta be low some grade of low temperature carbon steel.
Can you throw some light on the material selection??
Thanks in advance,
Timewrap.