What are the low temperature (-30 deg C) effects on ISO 898.1 Grade 8.8 bolts? ISO898.1 specifies a charpy impact strength of 30 J when tested to ISO 83, which I assume is conducted at a low temperature, but I don't know what that temperature is though. Any advise would be a great help.
 
Review ASME SecVIII Div1 UCS-66 and SecII A SF-568
 
ASTM A-320's are low temp. bolt
- depending on grade, they're 27J min(avg of 3);20J min (for any 1) specimen @ -101C or -73C

[Grade L1 is 54/41J @ -73C]
 