I have an application where I need to use anchor bolts at an ambient temperature of -44 Farenheidt. A-36 material is too brittle. Any suggestions?
 
ASTM A 320/A 320M – 02 Standard Specification for Alloy/Steel Bolting Materials for Low-Temperature Service.