Jul 9, 2007 #1 AUME99 Mechanical Joined Jul 9, 2007 Messages 2 Location US I have an application where I need to use anchor bolts at an ambient temperature of -44 Farenheidt. A-36 material is too brittle. Any suggestions?
I have an application where I need to use anchor bolts at an ambient temperature of -44 Farenheidt. A-36 material is too brittle. Any suggestions?
Jul 9, 2007 #2 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US ASTM A 320/A 320M – 02 Standard Specification for Alloy/Steel Bolting Materials for Low-Temperature Service. Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora. Upvote 0 Downvote