I am currently using an A-36 3" thick plate in a design. I would like to change the material type to include "Cobble Plate" or SMP - Stip Mill Plate. I was wondering on how you can esitmate the yield point of a material based on its chemical composition? Is there any good books out there on this? If I gave the chemical requirements that are following, would I be able to guarantee a certain min yield and what would it be?
Chemical Requirements:
Carbon: 0.05-0.33
Manganese: 0.25-1.35
Phosphorus: 0.04 (MAX)
Sulphur: 0.05 (MAX)