dear all,
with reference to ASME B31.3 Table 304.1.1 Values of Coefficient Y Low Alloy Material Like A335-P11 or A691 1.25Cr or A234-WP11 which is the group to take as reference for thickness calculation ? "Ferritic Steel" or "Other ductile metals" ?
thank for your supports
regards
 
Suggest that you repost on the "Piping, Pipelines and Fluid Mechnics Forum"