Just wanting to get some thoughts on the ASTM specifications for the two above properties - ASTM C150. It seems that the IR of 0.75% as given in ASTM is quite a bit on the low side - BS standards and Canadian standars permit up to 3% - Indonesian standards 5%. LOI is 5%, too, in Indonesia. Canada and BS are at 3% I think. It looks like we may have a hard time meeting ASTM for these two on our job. We are using relatively low strength mixes - RCC at 12 MPa at 1 year and normal concrete being maxed out at 30 MPa at 90 days. Any thoughts?