I am having a difficult time finding sources or vendors who sale Texaco Quenchtex or Shell Voluta Quench oils. I have called Texaco corporate to get the usual automated phone run around. No luck with Shell either. I am simply looking for a vendor who has one of the two so I can get a quote and make a purchase.
Thanks in advance for your help.

Nilcram
 
Replies continue below

Recommended for you

Large companies like Texaco and Shell distribute their products through a number of different channels. For example, independent companies like Alexis Oil sell Texaco products, including Quenchtex. Use the following link for more information:

 
Status