As per the topic title, I'm looking for an easier way to predict ferrite content in welds that to draw lines by hand on a copy of the Schaeffler/De Long, Bystram, WRC-92, ... diagrams.
I could make one in excel I suppose, however it's worth asking first to see if it doesn't yet exist.

Thanks!
 
It's not letting me upload the images I got from google, so I suggest you search there.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
That's exactly what I was looking for. Thanks!
 