Good afternoon,
I hope everyone is staying warm.
I'm searching for information on whether feature sizes will decrease or increase after anodizing.
I've heard both, that the feature size will increase and decrease, does this depend on the method of anodizing?
Looking at both Class I (AA-M12C22A44) and Class II (AA-M12C22A31) anodic coatings.
I understand that you build a layer of oxide on the surface of the base aluminum, but has the base aluminum been altered in size before the oxide is created.
All of your thoughts and opinions are welcomed .
Have a great day and thanks for your assistance in advance.
I hope everyone is staying warm.
I'm searching for information on whether feature sizes will decrease or increase after anodizing.
I've heard both, that the feature size will increase and decrease, does this depend on the method of anodizing?
Looking at both Class I (AA-M12C22A44) and Class II (AA-M12C22A31) anodic coatings.
I understand that you build a layer of oxide on the surface of the base aluminum, but has the base aluminum been altered in size before the oxide is created.
All of your thoughts and opinions are welcomed .
Have a great day and thanks for your assistance in advance.