The manufacturing differences are quite different and well documented in the literiture. Howewver, I believe your query relates to the advantages or disadvantages between the two.
One of the few or only advantage of sprial welded line pipe (and the reason for its emergence) is that it is generally less cost, and it can be produced at large diameters, at significantly less cost than longitudinal seamed line pipe.
The disadvantages of spiral welded line pipe are more significant, and have been a focus of considerable research and debate within the Industry for many years. Of most importance and concern is that the quality of the spiral weld can vary considerably amoungst manufacturers worldwide. The most agreed concern is the existance of stress concentrations in the spiral weld, since spiral welded pipe is not cold expanded during the manufacturing process.
In addition, the various design codes require that a joint factor be applied when computing the wall thickness based on internal pressure. The joint factor is dependent upon the material specification, and the "welding" procedure/method used to make the continous spiral weld (i.e. ERW, SAW, etc.)during manufacture.
Each Operating Company generally has their own position regarding use of spiral welded pipe on their projects. Some oil companies do not allow use spiral welded pipe for higher pressure service due to the poor past performance and experience with this type of pipe. Some Companies do not allow use of spiral welded pipe for "on-plot" piping/portions of pipelines inside facilities areas, but may allow use of it "off plot" outside the facilities plot limit boundaries.
There has always been two positions regarding the use of spiral welded line pipe. The people interested and driven by economics will promote the use of this line pipe (since it can be significantly less expensive), while the engineers are very cautious regarding the use of such pipe. I very much belong to the later group, since I have experienced the results of spiral welded pipe failures, resulting fires inside plant facilities, attributed to seam failure of spiral weld.
In addition, it is pointed out that that the maximum shear stress for restrained (buried) hot oil spiral welded pipe segments occurs along the spiral weld, who's orientaion is very close to a 45 degree angle to the pipe springline. This means that if there is significant shut-down and start up events of the line during the operational life, It is certain that fatigue of the spiral weld can be a consideration.