radair
Structural
- Nov 4, 2002
- 11
I was recently told that lock washers (a.k.a. split washers) were not allowed on A325 structural bolts. Their reasoning was the following in AISC's 9th Ed. of ASD (page 5-266):
"(e) Washers. Flat circular washers and square or rectangular beveled washers shall conform to the current requirements of ASTM Standard Specification for Hardened Steel washers, ASTM F436"
This reads to me that FLAT & BEVELED washers must be hardened steel washers, but I don't read this as a prohibition on lock washers. I can't understand why a contractor should remove these washers, particularly after seeing a recent failure due to ineffective Anco (lock) nuts.
Any opinions, preferably backed by spec.?
"(e) Washers. Flat circular washers and square or rectangular beveled washers shall conform to the current requirements of ASTM Standard Specification for Hardened Steel washers, ASTM F436"
This reads to me that FLAT & BEVELED washers must be hardened steel washers, but I don't read this as a prohibition on lock washers. I can't understand why a contractor should remove these washers, particularly after seeing a recent failure due to ineffective Anco (lock) nuts.
Any opinions, preferably backed by spec.?