About the only reason I can see coring beams is for concrete strength in high shear areas... for normal reinforcing percentages, strength has little impact on flexural strength. If high shear is the issue, then an area of low shear, neutral axis is OK.
Before you core, you should have a procedure in the event of 'failure' already laid out.
Dik