Load rating of reinforced concrete pipes is done by the pipe maufacturer. It forms a part of the pipe's specification. The grade of the pipe should be marked on or cast into the unit on manufacture. The load rating is dependant upon the grade of concrete utilised, the pipe wall thickness and the reinforcement quantity and location within the pipe structure.