Can anyone suggest any helpful liquid anti-corrosives that can be added to waternborne paints? The paints are to be applied to steel products.
 
Replies continue below

Recommended for you

Nitrites, silicates, molybdates,...organic filming inhibitors. It obviously depends on what the paint vehicle system can tolerate while still providing the required film forming properties.
 
Ref liquid inhibitors
They come with the product - but no matter what the literature tells you, the end result is only as good as the preparation. Better to look at that before getting too technical
 