TugboatEng
Marine/Ocean
I am looking for some insight into the cause of damage of these lip seals. I believe the material is FKM, shaft speeds are variable but can reach 600 feet per minute. Pressures are not more than a few feet H2O. Temperature ranges from ambient to not more than 150F. The fluid is gear oil or an emulsion of oil and water. The seals are providing satisfactory service but are severely damaged at the end of their expected life. The first picture is after 4 years in service and the second is 1 year.

