I'm new to gearing and have been doing a lot of reading. Any suggestions would be more than welcome.
We are designing a portable system for a military contract. Weight is very critical. In the system is a motor that generates 6 Nm up to 500 RPM. We are gearing this down to drive a cam that experiences up to 28 Nm continuous for 10 minutes at a time, operating on and off depending on load demands.
We've designed an 8:1 planetary gear set with MOD 2 profile, 16/50/116 tooth sun/planet/ring gears. Thickness is 12/13/12 mm to achieve adequate factors of safety. Planets will have lightening holes/pockets.
I'm interested first in possible finishes to protect the gear surfaces. We are considering PTFE filled hard anodize. Any thoughts or suggestions on that?
I'm also interested in a sanity check of our choices for gearing, particulalry if it strikes anyone out there that we're missing something.
Thanks in advance!
We are designing a portable system for a military contract. Weight is very critical. In the system is a motor that generates 6 Nm up to 500 RPM. We are gearing this down to drive a cam that experiences up to 28 Nm continuous for 10 minutes at a time, operating on and off depending on load demands.
We've designed an 8:1 planetary gear set with MOD 2 profile, 16/50/116 tooth sun/planet/ring gears. Thickness is 12/13/12 mm to achieve adequate factors of safety. Planets will have lightening holes/pockets.
I'm interested first in possible finishes to protect the gear surfaces. We are considering PTFE filled hard anodize. Any thoughts or suggestions on that?
I'm also interested in a sanity check of our choices for gearing, particulalry if it strikes anyone out there that we're missing something.
Thanks in advance!