franklin55
Mechanical
- Feb 19, 2009
- 40
There is a leakage from the nozzle of our urea reactor through weep holes (02 weep holes in the nozzle body), which indicate the liner inside is somewhere damaged. I am attaching its drawing too. The nozzle is attached to the top hemihead. Can somebody guide how to repair?