hi
i am having an issue with my laser cutting machine bystronic 3015
i cutting inox 4mm and while cutting the material,
the power of laser decreases till the next part it can't be cutted,
i have lowered the speed to obtain an acceptable cutting but this doesn't resolve the problem
can anyone help?
 
Sorry for the delay. open the top of the laser and see if the plasma stream degrades and gets stringy. Do a vacuum test.


Chris Krug Maximum Up-time, Minimum BS
 