Does anyone have experience cutting 4150 steel plate on a CO2 laser? I have a customer with 3 & 4Kw CO2 lasers that needs to quote a job from 8.5 mm (aprox 5/16 thick) plate. Any advice would be greatly appreciated.
 
Replies continue below

Recommended for you

I have previously cut with same settings as cutting 44w with very good results.
 