Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations Ron247 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

lamination test 1

Status
Not open for further replies.

maryam1979

Materials
Jul 17, 2005
11
Hi, is there anything in ASME about lamination test (UT) on plates over 20 mm in thickness?
 
Replies continue below

Recommended for you

I would suggest looking into MIL-STD-810, Labratory testing procedures.

Its not a detailed instruction, but gives a direction to go and you can fine tune it for your application.

Everett#2390
 
maryam,

It depends on what section of the ASME Code you are working with.

Section VIII Div 1 - no requirement
Section VIII Div 2 - AM-203 - UT if over 4"
Section III - NB-2531 - UT if over 2"

I am sure there are different requirements in other sections.