zacharialamsyah
Chemical
Dear All
I want to ask some topic which i'm not understand
1.What the differences between Lamellar Tear and Lamination? Because in some reference they are similar and not quite different?
2. Is it Z through test (through thickness test) can detect lamination also, beside its primary functions to detect lamellar tear?
3. If plate was detected have lamellar tear, what actions take to repair that plate, so the plate can reused?
Thank you for response and answer
Regards
Zachari Alamsyah
I want to ask some topic which i'm not understand
1.What the differences between Lamellar Tear and Lamination? Because in some reference they are similar and not quite different?
2. Is it Z through test (through thickness test) can detect lamination also, beside its primary functions to detect lamellar tear?
3. If plate was detected have lamellar tear, what actions take to repair that plate, so the plate can reused?
Thank you for response and answer
Regards
Zachari Alamsyah