KX2 1100 Bolt, what does it mean??

Status
Not open for further replies.

Aled87

Automotive
Joined
Mar 1, 2010
Messages
24
I have a bolt where the head is marked KX2 1100, does anybody have any specifications of this bolt. im trying to find ultimate tensile strengths and yeild strengths,

thank you
 
KX2 means the part was made by Kamax. The 1100 is not a standard designation, any chance that is an aluminium alloy screw made from AA 1100?
 
Alternatively, this could be a non-standard steel bolt with 1100 MPa nominal tensile strength.
 
If this is an automotive application, then it is almost certainly 1100 MPa ultimate tensile strength.
 