Feb 10, 2012 #1 Aled87 Automotive Joined Mar 1, 2010 Messages 24 I have a bolt where the head is marked KX2 1100, does anybody have any specifications of this bolt. im trying to find ultimate tensile strengths and yeild strengths, thank you
I have a bolt where the head is marked KX2 1100, does anybody have any specifications of this bolt. im trying to find ultimate tensile strengths and yeild strengths, thank you
Feb 10, 2012 #2 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US KX2 means the part was made by Kamax. The 1100 is not a standard designation, any chance that is an aluminium alloy screw made from AA 1100? Upvote 0 Downvote
KX2 means the part was made by Kamax. The 1100 is not a standard designation, any chance that is an aluminium alloy screw made from AA 1100?
Feb 13, 2012 #3 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US Alternatively, this could be a non-standard steel bolt with 1100 MPa nominal tensile strength. Upvote 0 Downvote
Feb 13, 2012 #4 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US If this is an automotive application, then it is almost certainly 1100 MPa ultimate tensile strength. Upvote 0 Downvote
If this is an automotive application, then it is almost certainly 1100 MPa ultimate tensile strength.