KX2 means the part was made by Kamax. The 1100 is not a standard designation, any chance that is an aluminium alloy screw made from AA 1100?
 
Alternatively, this could be a non-standard steel bolt with 1100 MPa nominal tensile strength.
 
If this is an automotive application, then it is almost certainly 1100 MPa ultimate tensile strength.
 