Ok, Thanks. Based on the literature you provided these are high temperature alloys which appear similar to Incoloy 800. So, I would recommend you visit the Special Metals alloy web site. The filler metal that would be compatible for Incoloy 800 is Inco-Weld A for the SMAW process. I would strongly recommend you qualify a weld procedure for the above base materials and nickel-base filler metals to ensure no weldability concerns.