Dec 16, 2004 #1 soya Mechanical Joined Dec 9, 2004 Messages 11 Location GB Dear friends, Could anyone let me know how to get the Jominy Test data(eg the position of the specimen and the response temperature together with the time)? Thanks.
Dear friends, Could anyone let me know how to get the Jominy Test data(eg the position of the specimen and the response temperature together with the time)? Thanks.
Dec 16, 2004 #2 EdStainless Materials Joined May 20, 2004 Messages 16,379 Location Waukesha WI USA ASTM A255 covers the setup and test method. Timken publishes a great little book of Jominy data. = = = = = = = = = = = = = = = = = = = = Corrosion never sleeps, but it can be managed. http://www.trenttube.com/Trent/tech_form.htm Upvote 0 Downvote
ASTM A255 covers the setup and test method. Timken publishes a great little book of Jominy data. = = = = = = = = = = = = = = = = = = = = Corrosion never sleeps, but it can be managed. http://www.trenttube.com/Trent/tech_form.htm
Dec 16, 2004 #3 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Another option is SAE J406 specification - Methods for Determining Hardenability of Steels http://www.sae.org/servlets/productDetail?PROD_TYP=STD&PROD_CD=J406_199805 Upvote 0 Downvote
Another option is SAE J406 specification - Methods for Determining Hardenability of Steels http://www.sae.org/servlets/productDetail?PROD_TYP=STD&PROD_CD=J406_199805