Is there a direct JIS equivalent for SAE 1010-1020 HSLA steel? Also, if I only have the JIS steel spec #, how do I translate that to the SAE equivalent?
 
1010-1020 is not HSLA.

The numbers 1010-1020 only refer to chemistry according to SAE J403.

Most JIS standards are for specific product forms (sheet, bar, etc.).

Can you provide more information?

As for translating specfications, there is no easy method. Perform a search at this site for references (like Stahlschlussel or Worldwide Guide to Equivalent Irons and Steels)

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
1010-1020 is not HSLA.
ASTM 1010~JIS S10C
ASTM 1020~JIS S20C

Regards
 