I am working with a 303 SS jack screw with M5 threads. The connector mating load is predicted to be about 20 pounds. The torque I have specified is 10 inch-pounds.
My problem is I am failing the extrenal threads in a short amount of time (25-30) matings. Do you reccomend alternative stainless steels as well as any lubricants? If so, what type of lube? Thank you in advance, Bill B.
William H. Bernhart, P.E.
I work as a development engineer for AMP - Tyco Electronics located near Harrisburg, PA. I help design interconnections and electrical connectors for aerospace applications.
I am working with a 303 SS jack screw with M5 threads. The connector mating load is predicted to be about 20 pounds. The torque I have specified is 10 inch-pounds.
My problem is I am failing the extrenal threads in a short amount of time (25-30) matings. Do you reccomend alternative stainless steels as well as any lubricants? If so, what type of lube? Thank you in advance, Bill B.