I am reading a hydrogen embrittlement research paper put out by Republic Steel (it is a reprint of a Kobe paper) and there is a section on phosphate wire rod coatings causing embrittlement in heat treated bolts made from said rod. There is a photomicrograph purporting to show a 12 micron phosphorus rich layer on the surface of the sample. And, the paper cites ISO 898-1-1988 as prohibiting a white phosphorus enriched layer on heat treated bolts.Anyone ever heard of this?