what is meant by supply condition in iso 13847 clause 7.6.3.3 Supply condition
shall i perform a separate wpqr for each type of fitting (flange , elbow , tee , weldolet)
 
Heat treated, cold worked, etc etc. The material condition rather than the product form.

Steve Jones
Corrosion Management Consultant