Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ISO 10042_weld aluminium alloy standard do not mention about weld penetration???

Status
Not open for further replies.

Ryan.z

Mechanical
Joined
Dec 17, 2021
Messages
4
Location
VN
Hi you guys

I have a question about welding imperfections standard ISO 10042. In this document do not mention about welding penetration.
To judge welding defect: lack of penetration lever C, h< 0.2s but this document do not mention how much of "s" value?
lackfusion_o8v2l6.png


and about penetration size as well as, this document no not say how much of "h2" and "h6" value, this is penetration value
penetration_yp3yf9.png


How can I judge the lack of penetration defect base on iso 10042?
 
S should be taken from the plans or drawings (nominal value, see § 4).
For multiple imperfections, h2 and h6 refer to the lack of penetration but in practice this is for butt welds, I've never seen this applied for fillet welds.
 