Dear all,
I had just received a photo of the failed shaft's fractured surface and I was wondering if this fracture surface is caused by shear or fatigue. I had asked our mentor regarding this and he claimed that it was caused by fatigue due to the fact that there were ratchet marks at the left side of the shaft. Seriously, I am not convinced.
I had just received a photo of the failed shaft's fractured surface and I was wondering if this fracture surface is caused by shear or fatigue. I had asked our mentor regarding this and he claimed that it was caused by fatigue due to the fact that there were ratchet marks at the left side of the shaft. Seriously, I am not convinced.