Is there an equivalent to ASTM D-930 and ASTM D1280?

JoeBobJenkins

Marine/Ocean
Mar 7, 2006
28
I've got instructions stating I need to test aluminum corrosion limits for a cleaner IAW ASTM D-930 or ASTM D-1280. Problem is both of these have been withdrawn and not superceded. I can't seem to find a replacement or equivalent for either. Any hints?
 
Replies continue below

Recommended for you

The last published versions are still available, and they still define methods of test that are executable.

You could contact ASTM and ask for the relevant committee meeting minutes, they should document the reason for the withdrawal, and might point to alternatives.
 