Dear Friends
Project - Conversion of Tanker Vesel into FPSO Platform
Material Group 1- ASTM A106-B x 6" x 21.95thk ( Process Piping )
Weld Process - GTAW / SMAW. Applicable Code-ASME B31.3
Upon completion of PWHT/Hardness Test , RT Done- It passed. Did not do MPI.
The purpose of MPI is to detect Surface/Sub-Surface Discontinuities which could be missed out by RT.
But here I'm working with Plain Carbon Steel.
Is it mandatory to do MPI?. Where I can find this requirement in ASME B31.3 or in any other ASME codes.
I'ne gone through Chapter VI, but found nothing about MPI Requirement after PWHT(Stress Relief )
Appreciate prompt guidance and advise
Project - Conversion of Tanker Vesel into FPSO Platform
Material Group 1- ASTM A106-B x 6" x 21.95thk ( Process Piping )
Weld Process - GTAW / SMAW. Applicable Code-ASME B31.3
Upon completion of PWHT/Hardness Test , RT Done- It passed. Did not do MPI.
The purpose of MPI is to detect Surface/Sub-Surface Discontinuities which could be missed out by RT.
But here I'm working with Plain Carbon Steel.
Is it mandatory to do MPI?. Where I can find this requirement in ASME B31.3 or in any other ASME codes.
I'ne gone through Chapter VI, but found nothing about MPI Requirement after PWHT(Stress Relief )
Appreciate prompt guidance and advise