Now, pure air that these tanks collect, is, pretty much non-corrosive...... however,
the condensate that collects in the bottom of every single air receiver,....... Well, that is very corrosive !
Based on research I have conducted at Lowes and Home Depot, I believe that, below a certain volume, inspection openings may be deleted
Sekar, what kind of tank volumes, pressures and diameters interest you ?
MJCronin
Sr. Process Engineer