Hi guys,
I'm working on a carbon steel vessel with MDMT of -24degree C, the shell material is ASTM A516 Gr70 and the forgings/flanges are A105. I understand ASME B16.5 flanges are excepted from impact testing up to -29degree C. I've got a heavy neck forging of 152.4mm thk welded into the 35mm thk plate. I've carried out a preliminary calc as per UCS-66 which is indicating it being excepted.
Can someone throw more light or ref me to the relevant section.
tr (required thickness of forging neck) = 4.961mm
tn (norminal thickness of forging neck) = 152.4mm
E (joint efficiency) = 0.85
C (corrosion allowance) = 0
Many Thanks in advance.
Fizzy
I'm working on a carbon steel vessel with MDMT of -24degree C, the shell material is ASTM A516 Gr70 and the forgings/flanges are A105. I understand ASME B16.5 flanges are excepted from impact testing up to -29degree C. I've got a heavy neck forging of 152.4mm thk welded into the 35mm thk plate. I've carried out a preliminary calc as per UCS-66 which is indicating it being excepted.
Can someone throw more light or ref me to the relevant section.
tr (required thickness of forging neck) = 4.961mm
tn (norminal thickness of forging neck) = 152.4mm
E (joint efficiency) = 0.85
C (corrosion allowance) = 0
Many Thanks in advance.
Fizzy