rollingcloud
Aerospace

The material is UNS S42716. It was supposed to be heated to 1925 °F (1052 °C), held at heat for 30 minutes, quenched in oil, sub-zero cooled to -100 °F (-73 °C), held for 2 hours, warmed in air to room temperature and tempered at 350 °F (177 °C) for an hour.
Is the black discoloration a heat scale? I was told that the ones on the left are not an issue and its only cosmetic. However, the one on the right looks much worse. The finish requirement is 32 Ra, would the scale make the surface too rough? Does it decrease the corrosion resistance?