is f6nm steel brittle or ductile material?
 
At what C level? What strength? What temperature?
In general this a fairly tough material but it has its limits.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
It will be somewhere in between; precisely where depends on the quality and the heat treat condition.
No metallic alloy is truly 'brittle', metals just have varying degrees of ductility.