Anyone help me,

whatis voltage level to check insulation resistance for anode with cable and earth for cathodic protection.,nomaly this anode for positive ptention from rectifier 50V.

Thank
 
Replies continue below

Recommended for you

If you intend to test the insulation resistance of the cable you have to be sure the anode end is dry and the connection box end disconnected and then for a rated cable of 600 V [HMWPE] minimum resistance measurer with a tester of 500 V could be 2 megohm .See for instance:
But you don't have to test the IR of the cable. In order to test the cathodic protection system see:
The IR test on completed [new] cable in the manufacturer shop will be according to
ANSI/NEMA WC 70-2009/ICEA S-95-658-2009 ch.6.10.2 Insulation Resistance.
 