Aug 3, 2015 #1 BoltSlinger Industrial Joined Jun 24, 2015 Messages 11 Location US anyone know any type of bar I can get with a carbon range of 70% to 82%? Thank you!
Aug 3, 2015 #2 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US I assume you mean steel bar with carbon concentration of 0.70 to 0.82 percent by mass. If so, then grade 1070 or 1080 should be suitable for your needs. Summit Steel is one potential supplier: http://www.summitsteel.com/steel-bar-products/ Upvote 0 Downvote
I assume you mean steel bar with carbon concentration of 0.70 to 0.82 percent by mass. If so, then grade 1070 or 1080 should be suitable for your needs. Summit Steel is one potential supplier: http://www.summitsteel.com/steel-bar-products/