First post.
I just did a reverse engineering of a splined hub I need to replicate (different driveline).
Certainly metric, I deduced that the spline were 30 degrees, with a module of 1mm and 12 teeth. I measured the shaft and hub diameters over pins according to DIN5480 (2.5mm for the shaft, 1.75mm for the hub) to be as follow:
17.23mm@2.5mm
10.56mm@1.76mm
Using Kisssoft and DIN5480, I found out it was not actually the default profile shift 0.45mm. Therefore, I used the above measurement to compute a new profile shift coef. of .555mm. Measurement over pins now checks out.
However, the tip and root diameter are way off for both the shaft and hub.
Shaft root is measured at 11.20mm instead of designed 12.01mm.
Shaft tip is measured at 13.75 instead of 14.01mm.
Hub tip is measured at 13.96mm instead of designed 14.22mm.
Hub root is measured at 12.08mm instead of designed 12.21mm.
The splines may be JIS. 1. Could this explain the difference? Kisssoft does not have the JIS standard integrated.
2. Does it matter? My understanding is that they will fit properly if the diameter over pin is right. 3. Should I change my hub diameters or let them as designed?
Thank you for your help?
I just did a reverse engineering of a splined hub I need to replicate (different driveline).
Certainly metric, I deduced that the spline were 30 degrees, with a module of 1mm and 12 teeth. I measured the shaft and hub diameters over pins according to DIN5480 (2.5mm for the shaft, 1.75mm for the hub) to be as follow:
17.23mm@2.5mm
10.56mm@1.76mm
Using Kisssoft and DIN5480, I found out it was not actually the default profile shift 0.45mm. Therefore, I used the above measurement to compute a new profile shift coef. of .555mm. Measurement over pins now checks out.
However, the tip and root diameter are way off for both the shaft and hub.
Shaft root is measured at 11.20mm instead of designed 12.01mm.
Shaft tip is measured at 13.75 instead of 14.01mm.
Hub tip is measured at 13.96mm instead of designed 14.22mm.
Hub root is measured at 12.08mm instead of designed 12.21mm.
The splines may be JIS. 1. Could this explain the difference? Kisssoft does not have the JIS standard integrated.
2. Does it matter? My understanding is that they will fit properly if the diameter over pin is right. 3. Should I change my hub diameters or let them as designed?
Thank you for your help?