Is there a DIN, BS, EN, JIS or other common dimensional standard equivalent or comparable to ASME B16.11 for forged fittings?

I hope someone with broader horizons than myself can answer without expending more than a few seconds. My google searches and the reference books I have didn't turn up anything in the first 10 minutes.

- Steve Perry
This post is designed to provide accurate and authoritative information in regard to the subject matter covered. It is offered with the understanding that the author is not engaged in rendering engineering or other professional service. If you need help, get help, and PAY FOR IT.
 
Replies continue below

Recommended for you

... and as a follow up, how prevalent are these versus ASME B16.11 fittings?

- Steve Perry
This post is designed to provide accurate and authoritative information in regard to the subject matter covered. It is offered with the understanding that the author is not engaged in rendering engineering or other professional service. If you need help, get help, and PAY FOR IT.
 
•DIN 2615-2:1992
Steel butt-welding pipe fittings; tees for use at full service pressure
•DIN 2616-2:1991
Steel butt-welding pipe fittings; reducers for use at full service pressure
•DIN 2617:1991
Steel butt-welding pipe fittings; caps
•DIN 2618:1968
Butt welding steel fittings; welding saddles, nominal pressure
•DIN 2619:1968
Butt welding steel fitting; bends for welding, nominal pressure 16

"And as a follow up, how prevalent are these versus ASME B16.11 fittings?" That just depends on the client, location and project. I've had some projects where one area is DIN and other area is ASME/ANSI. Make the connection with a pipe in the middle.

What would you be doing, if you knew that you could not fail?
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor