I have seen 24" listed as the maximum size for A234 WPB (seamless) fittings; beyond that they are welded (WPB-W).
Is there a standard that actually specifies this as as the breakpoint?
Additionally, their pressure ratings should both be equivalent to seamless pipe if built to B16.9 (para 2.1). It seems like it would make more sense to be able to specify an A234 WPB fitting of either construction but A234 does not allow this option as WPB by itself indicates seamless. Maybe there are other requirements triggered by use of welded fittings I'm not considering?
Thanks in advance
Is there a standard that actually specifies this as as the breakpoint?
Additionally, their pressure ratings should both be equivalent to seamless pipe if built to B16.9 (para 2.1). It seems like it would make more sense to be able to specify an A234 WPB fitting of either construction but A234 does not allow this option as WPB by itself indicates seamless. Maybe there are other requirements triggered by use of welded fittings I'm not considering?